Sign In | Join Free | My himfr.com
Home > Thermal Spray Powders >

WC-12Ni HVOF Powder Wear Resistant Equal To WOKA 3401 WOKA 3402 WOKA 3403 WOKA 3404 WOKA 3306 WOKA 3408

Zhuzhou Jiangwu Boda Hard-Facing Materials Co., Ltd.
Trust Seal
Verified Supplier
Credit Check
Supplier Assessment
Contact Now
    Buy cheap WC-12Ni HVOF Powder Wear Resistant Equal To WOKA 3401 WOKA 3402 WOKA 3403 WOKA 3404 WOKA 3306 WOKA 3408 from wholesalers
     
    Buy cheap WC-12Ni HVOF Powder Wear Resistant Equal To WOKA 3401 WOKA 3402 WOKA 3403 WOKA 3404 WOKA 3306 WOKA 3408 from wholesalers
    • Buy cheap WC-12Ni HVOF Powder Wear Resistant Equal To WOKA 3401 WOKA 3402 WOKA 3403 WOKA 3404 WOKA 3306 WOKA 3408 from wholesalers

    WC-12Ni HVOF Powder Wear Resistant Equal To WOKA 3401 WOKA 3402 WOKA 3403 WOKA 3404 WOKA 3306 WOKA 3408

    Ask Lasest Price
    Brand Name : BODA
    Model Number : BD-10502
    Certification : ISO9001:2015,ISO14001
    Price : US$51.80/kg-$53.50/kg EX-WORK
    Payment Terms : T/T
    Supply Ability : 10-15 tons per month
    Delivery Time : 5-8 working days
    • Product Details
    • Company Profile

    WC-12Ni HVOF Powder Wear Resistant Equal To WOKA 3401 WOKA 3402 WOKA 3403 WOKA 3404 WOKA 3306 WOKA 3408

    WC-12Ni HVOF Powder Wear Resistance Equal To WOKA 3401 WOKA 3402 WOKA 3403 WOKA 3404 WOKA 3306 WOKA 3408

    BODA WC-12Ni products are spheroidal, agglomerated and sintered powders for thermal spray containing a uniform distribution of 88 % tungsten carbide with medium sized carbide grains as a hard phase and 12 % nickel as a binder metal.
    The finer powder particle size distributions produce very tough and dense coatings that can often be used in the “as-
    sprayed” condition without post-coat finishing.Coatings made from tungsten carbide materials resist fret-
    ting, abrasion, hammer and sliding wear. BODA WC-12Ni series products are most often used for abrasion-resistant coatings in dry environments. Their use at atmospheric temperatures
    above 500 °C (930 °F) is not recommended to prevent oxi-
    dation of the tungsten carbide. The corrosion resistance of WC-Ni is generally better than that of WC-Co coatings in
    similar environments, but not as good as coatings of WC-Co-Cr. BODA WC-12Ni coatings exhibit higher hard-ness compared to coatings of WC-17Ni, but have lower toughness. They have lower hard-
    ness but better toughness than coatings from WC-10Ni. The absence of cobalt allows
    BODA WC-12Ni coatings to be used in radioactive environments.
    HVOF coatings of these materials are dense, show good
    bond strength and are more homogeneous than coatings
    applied using atmospheric plasma spray or combustion
    powder Thermospray ™ coatings.

    Typical Uses and Applications
    Ball valves in oxidizing environments
    Gate valves
    Oil field equipment
    Parts used in submerged seawater conditions


    Quality WC-12Ni HVOF Powder Wear Resistant Equal To WOKA 3401 WOKA 3402 WOKA 3403 WOKA 3404 WOKA 3306 WOKA 3408 for sale
    Inquiry Cart 0
    Send your message to this supplier
     
    *From:
    *To: Zhuzhou Jiangwu Boda Hard-Facing Materials Co., Ltd.
    *Subject:
    *Message:
    Characters Remaining: (0/3000)